Welding Procurection Qualification (Welding Procurection Qualification, ake magana a kai a matsayin WPQ) shine tsarin gwajin da sakamakon sakamako don tabbatar da daidaito na tsarin walda da aka gabatar.

Tabbatar da aikin walda muhimmin ma'auni ne don tabbatar da inganci da samar da abin dogaro da tushe don ƙirƙirar umarnin aikin walda ko katunan aikin walda.

I. Pturawa

1. Tantance ko sashin walda yana da ikon haɗa walda wanda ya dace da buƙatun ƙa'idodin ƙasa ko masana'antu masu dacewa da ƙwarewar fasaha;

2. Tabbatar cewa tsarin aikin walda (WPS ko pWPS) wanda sashin walda ya zana daidai ne.

3. Samar da ingantacciyar hanyar fasaha don ƙirƙirar umarnin aikin walda na yau da kullun ko katunan aikin walda.

II. Sƙyama

Welding tsari muhimmin ma'auni ne don tabbatar da ingancin walda. Zai iya tabbatar da daidaito da hankali na jagororin aikin walda waɗanda aka shirya don ɗakunan mahaɗa daban-daban. Ta hanyar cancantar aikin walda, duba ko aikin aikin walda da walda ya yi daidai da daftarin littafin wajan tsarin wajan ya cika bukatun zane, kuma ya samar da abin dogaro da abin dogaro ga tsarin kirkira na littafin aikin walda ko katin walda.

III. Yanayin aikace-aikace

1. Ya dace da ƙera, sakawa da kuma kula da kayan aikin ƙarfe kamar tukunyar jirgi, jiragen ruwa na matsi, bututun matsewa, gadoji, jiragen ruwa, kumbon sama, makamashin nukiliya da sifofin ƙarfe masu ɗaukar kaya

2. Ya dace da hanyoyin walda kamar walda na gas, walda na walda, argon tungsten arc waldi, walkin karfe karfe, waldi na karkashin ruwa, walkin plasma arc, da walda na electroslag.

IV. Tsari

1. Welding hanya cancantar

2. Bayar da abubuwa don cancantar aikin walda

3. Tsara waldi tsari tsari

4. Welding hanya cancantar gwajin

5. Shirye-shiryen rahoton cancantar aikin walda

6. Haɗuwa da tsarin aikin walda dalla-dalla (umarnin aiki don katunan aiki da katunan aiki)

V. Tsarin kimantawa

1. Tsara Tsarin Welding na farko (pWPS)

2. Welding gwajin guda da samfurin shiri

3. Gwajin gwaje-gwaje da samfurori

4. ayyade ko haɗin da aka yi wa walda ya sadu da aikin da ake buƙata ta daidaitacce

5. Submitaddamar da rahoton cancantar aikin walda don tantance tsarin aikin walda da aka gabatar

VI. Kimantawa standards

Daidaitacce Sinanci ka'idoji don kimanta tsari

1 NB / T47014-2011 “Ingancin hanyoyin walda don kayan matsi”

2 GB5023698 "Kayan Field, Ginin Injin Welding Injiniyan Injiniyanci da Matakan Bincike Na Matsi"

3 "Dokokin Kulawa da Kayan Karkataccen Tukunyar Steam (1996)" Lura: Ana amfani da wannan ƙa'idar don kimanta tsari a masana'antar ɗaga kayan

4 SY ∕ T0452-2002 "Hanyar Inganta Hanyar Inganta Man Fetur da Gas Gas" (Lura: don cancantar aikin mai da sinadarai)

5 GB50661-2001 "Musammantawa don Welding na Karfe Tsarin" (Lura: Koma zuwa aiwatar da aikin kimantawa da babbar hanyar gadoji)

6 SY ∕ T41032006 "Karfe bututu Welding da Yarda"

7. JB4708-2000 "Ingancin Ka'idojin Welding don Matakan Jirgin Karfe".

Matsayin Turai

EN 288 ko ISO 15607-ISO 15614 mizanin jeri

ISO15614-1 Arc waldi da waldi na karfe / Arc waldi na nickel da nickel gami

ISO15614-2 Arc waldi na aluminum da aluminum gami

ISO15614-3 baƙin ƙarfe baka

Gyara waldi na ISO15614-4 yaye aluminum

ISO15614-5 Walc na titanium da guntun titin gami / arc walda na zirconium da zirconium gami

ISO15614-6 Arc waldar tagulla da tagulla

ISO15614-7 waldi mai walƙiya

Welding na ISO15614-8 bututun mahaɗa da haɗin bututun ƙarfe

Matsayin Amurka

1.AWS

D1.1 ∕ D1.1M: 2005 Karfe tsarin walda bayani dalla-dalla

D1.2 ∕ D1.2M: Tsarin walda na 2003 don tsarin aluminum

D1.3-98 eldayyadaddun walda don tsarin bakin karfe

D1.5 ∕ D1.5M: Wurin walda na 2002

D1.6: 1999 Bakin karfe waldi

D14.3 ∕ D14.3M: Dokokin Welding na Wuraren 2005


Post lokaci: Apr-14-2021